Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP CP GFR 20 FR V0 EMAS Plastik San.Tic.AS.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | EMAS Plastik San.Tic.AS./CP GFR 20 FR V0 |
---|---|---|---|
Impact strength of cantilever beam gap | ISO 180/1A | >8.0 kJ/m² |
hardness | Test Condition | Test Method | EMAS Plastik San.Tic.AS./CP GFR 20 FR V0 |
---|---|---|---|
Shore hardness | 邵氏D | ISO 868 | 65to70 |
Mechanical properties | Test Condition | Test Method | EMAS Plastik San.Tic.AS./CP GFR 20 FR V0 |
---|---|---|---|
Tensile modulus | ISO 527-2 | 4000to7500 MPa | |
Tensile strain | 断裂 | ISO 527-2 | >4.0 % |
tensile strength | 屈服 | ISO 527-2 | 50.0to80.0 MPa |
flammability | Test Condition | Test Method | EMAS Plastik San.Tic.AS./CP GFR 20 FR V0 |
---|---|---|---|
UL flame retardant rating | UL 94 | V-0 | |
Hot filament ignition temperature | VDE0471/2 | 960 °C |
physical property | Test Condition | Test Method | EMAS Plastik San.Tic.AS./CP GFR 20 FR V0 |
---|---|---|---|
Shrinkage rate | 0.35to0.55 % | ||
density | ISO 1183 | 1.24to1.30 g/cm³ | |
melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 3.0to18 g/10min |
Thermal performance | Test Condition | Test Method | EMAS Plastik San.Tic.AS./CP GFR 20 FR V0 |
---|---|---|---|
vicat | ISO 306/B | 110 °C | |
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 110 °C |
melting temperature | ISO 3146 | 160 °C |