Mechanical properties | Test Condition | Test Method | DENKA JAPAN/SR-T-7H |
---|---|---|---|
Flexural modulus | ASTM-D790 | 2400 Mpa | |
Impact strength of cantilever beam gap | ASTM-D256 | 363 J/m | |
Rockwell hardness | ASTM-D785 | 106 R-Scale | |
tensile strength | ASTM-D638 | 45 Mpa | |
bending strength | ASTM-D790 | 65 Mpa |
physical property | Test Condition | Test Method | DENKA JAPAN/SR-T-7H |
---|---|---|---|
Shrinkage rate | ASTM-D955 | 0.4-0.6 % |
Thermal performance | Test Condition | Test Method | DENKA JAPAN/SR-T-7H |
---|---|---|---|
vicat | 200℃/5kg | ASTM-D1525 | 97 °C |
Heat distortion temperature | 18.6kg/cm,HDT | ASTM-D648 | 86 °C |
UL flame retardant rating | UL 94 | HB calss |