Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA12 3030JI5 UBE JAPAN
UBESTA
pipeline、Automotive sector、Pipe fittings
Thermal stability、Easy to process、High impact resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | UBE JAPAN/3030JI5 |
---|---|---|---|
Shore hardness | 邵氏D | ISO 868 | 67 |
Rockwell hardness | R计秤 | ISO 2039-2 | 51 |
Mechanical properties | Test Condition | Test Method | UBE JAPAN/3030JI5 |
---|---|---|---|
bending strength | ISO 178 | 19.0 Mpa | |
Flexural modulus | ISO 178 | 400 Mpa | |
Tensile strain | 断裂 | ISO 527-2 | 200 % |
屈服 | ISO 527-2 | 24 % | |
tensile strength | 屈服 | ISO 527-2 | 26.0 Mpa |
Electrical performance | Test Condition | Test Method | UBE JAPAN/3030JI5 |
---|---|---|---|
Volume resistivity | IEC 60093 | 1E+12 ohms·cm |
physical property | Test Condition | Test Method | UBE JAPAN/3030JI5 |
---|---|---|---|
Shrinkage rate | TD | ISO 294-4 | 1.4 % |
MD | ISO 294-4 | 0.70 % | |
melt mass-flow rate | 235°C/2.16kg | ISO 1133 | 4.0 g/10min |
Water absorption rate | 23°C,24hr | ISO 62 | 0.60 % |
Thermal performance | Test Condition | Test Method | UBE JAPAN/3030JI5 |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 91.0 °C |
1.8MPa,未退火,HDT | ISO 75-2/A | 45.0 °C | |
Linear coefficient of thermal expansion | MD | ISO 11359-2 | 1.7E-04 cm/cm/°C |
melting temperature | ISO 3146 | 173 °C |