PC 8600 STYRON TAIWAN
EMERGE™
--
Flame retardant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | STYRON TAIWAN/8600 |
---|---|---|---|
Dart impact | 23°C,3.20mm,注塑,总能量 | ASTM D3763 | 58.8 J |
hardness | Test Condition | Test Method | STYRON TAIWAN/8600 |
---|---|---|---|
Rockwell hardness | R级,3.20mm,注塑 | ASTM D785 | 123 |
Mechanical properties | Test Condition | Test Method | STYRON TAIWAN/8600 |
---|---|---|---|
tensile strength | 屈服,3.20mm,注塑 | ASTM D638 | 60.0 Mpa |
elongation | 断裂,3.20mm,注塑 | ASTM D638 | 110 % |
Flexural modulus | 3.20mm,注塑 | ASTM D790 | 2400 Mpa |
elongation | 屈服,3.20mm,注塑 | ASTM D638 | 6.2 % |
tensile strength | 断裂,3.20mm,注塑 | ASTM D638 | 57.9 Mpa |
bending strength | 3.20mm,注塑 | ASTM D790 | 93.8 Mpa |
Tensile modulus | 3.20mm,注塑 | ASTM D638 | 2210 Mpa |
flammability | Test Condition | Test Method | STYRON TAIWAN/8600 |
---|---|---|---|
UL flame retardant rating | 3.00mm | UL 94 | V-0 |
1.50mm | UL 94 | V-0 | |
Burning wire flammability index | 1.00mm | IEC 60695-2-12 | 960 °C |
Limiting Oxygen Index | ASTM D2863 | 35 % |
physical property | Test Condition | Test Method | STYRON TAIWAN/8600 |
---|---|---|---|
Shrinkage rate | MD | ASTM D955 | 0.50-0.70 % |
melt mass-flow rate | 300°C/1.2kg | ASTM D1238 | 7.0 g/10min |
Thermal performance | Test Condition | Test Method | STYRON TAIWAN/8600 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | 127 °C |
RTI | 3.20mm | UL 746 | 125 °C |
Heat distortion temperature | 0.45MPa,未退火,HDT | ASTM D648 | 139 °C |
RTI Elec | 3.20mm | UL 746 | 125 °C |
vicat | ASTM D15252 | 149 °C | |
Linear coefficient of thermal expansion | MD:-40到82°C | ASTM D696 | 6.5E-05 cm/cm/°C |
RTI Imp | 3.20mm | UL 746 | 125 °C |