ETFE 750 CHEMOURS US
TEFZEL®
Electric wire,Cable Applications,Electronic insulation,Electrical field,Electronic field
Low friction coefficient,copolymer,Processability,Good flexibility,Chemical resistance,heat-resisting,High toughness
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | CHEMOURS US/750 |
|---|---|---|---|
| Melting temperature | ASTM D3159 | 219to254 °C |
| mechanical properties | Test Condition | Test Method | CHEMOURS US/750 |
|---|---|---|---|
| Bending modulus | ASTM D790 | 645 Mpa | |
| elongation | Break,180°C | ASTM D1708 | 600 % |
| Break,160°C | ASTM D1708 | 650 % | |
| Break,23°C | ASTM D1708 | 300 % | |
| Break,140°C | ASTM D1708 | 600 % | |
| Break,200°C | ASTM D1708 | 600 % | |
| tensile strength | 180°C | ASTM D1708 | 6.21 Mpa |
| 140°C | ASTM D1708 | 11.4 Mpa | |
| 200°C | ASTM D1708 | 3.45 Mpa | |
| 23°C | ASTM D1708 | 37.9 Mpa | |
| 160°C | ASTM D1708 | 8.62 Mpa |
| Physical properties | Test Condition | Test Method | CHEMOURS US/750 |
|---|---|---|---|
| melt mass-flow rate | 297°C/5.0kg | ASTM D3159 | 7.0 g/10min |
| flammability | Test Condition | Test Method | CHEMOURS US/750 |
|---|---|---|---|
| Extreme Oxygen Index | ASTM D2863 | 34 % |