PA66 S223-G6U DSM HOLAND
Akulon®
--
enhance,Glass fiber reinforced
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Mechanical properties | Test Condition | Test Method | DSM HOLAND/S223-G6U |
---|---|---|---|
Tensile modulus | 1mm/min | ISO 527-1 | 10000 MPa |
fracture strain | 5mm/min | ISO 527-1 | 3.5 % |
Impact strength of cantilever beam gap | 23℃ | ISO 180/1C | 65 KJ/m |
23℃ | ISO 180/1A | 13 KJ/m | |
Breaking stress | 5mm/min | ISO 527-1 | 195 MPa |
Electrical performance | Test Condition | Test Method | DSM HOLAND/S223-G6U |
---|---|---|---|
dielectric constant | 50Hz | IEC 60250 | 3.9 |
Volume resistivity | IEC 60093 | 1E+15 Ohm.cm | |
Surface Resistivity | IEC 60093 | 1E+15 Ohm | |
dielectric constant | 1MHz | IEC 60250 | 3.5 |
Dielectric loss | 1MHz | IEC 60250 | 160 E-4 |
50Hz | IEC 60250 | 90 E-4 |
physical property | Test Condition | Test Method | DSM HOLAND/S223-G6U |
---|---|---|---|
Water absorption rate | 23℃,50%相对湿度 | ISO 62 | 1.6 % |
density | ISO 1183 | 1.36 g/cm |
Thermal performance | Test Condition | Test Method | DSM HOLAND/S223-G6U |
---|---|---|---|
Heat distortion temperature | 0.45,HDT | ISO 75-2 | 260 ℃ |
1.8Mpa,HDT | ISO 75-2 | 250 ℃ | |
UL flame retardant rating | UL94 | HB |