| mechanical properties | Test Condition | Test Method | TEIJIN JAPAN/1225R BK |
|---|---|---|---|
| bending strength | ISO 178 | 92 Mpa | |
| Tensile strain | YieldYield | ISO 527-1-2 | 6 Mpa |
| tensile strength | Yield | ISO 527-1-2 | 62 Mpa |
| Bending modulus | ISO 178 | 2350 Mpa | |
| tensile strength | Break | ISO 527-1-2 | >50 Mpa |
| flame retardant performance | Test Condition | Test Method | TEIJIN JAPAN/1225R BK |
| UL flame retardant rating | 1.90 mm | UL 94 | HB |
| 0.40 mm | UL 94 | V-2 | |
| Physical properties | Test Condition | Test Method | TEIJIN JAPAN/1225R BK |
| density | ISO 1183 | 1.2 g/cm³ | |
| Shrinkage rate | MD | Internal Method | 0.5 - 0.7 % |
| TD | Internal Method | 0.5 - 0.7 % | |
| Melt Volume Flow Rate (MVR) | ISO 1133 | 11 cm3/10min | |
| thermal performance | Test Condition | Test Method | TEIJIN JAPAN/1225R BK |
| Hot deformation temperature | 1.8 MPa | ISO 75-1/2 | 128 °C |
| impact performance | Test Condition | Test Method | TEIJIN JAPAN/1225R BK |
| Charpy Notched Impact Strength | ISO 179 | NB kJ/m² |