Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PUR 800 AP/442 USA Anderson
--
--
Solubility resistance and hydrolysis stability
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Other performance | Test Condition | Test Method | USA Anderson/800 AP/442 |
---|---|---|---|
STORAGE STABILITY | 5.0 to 8.0 min |
Test Condition | Test Method | USA Anderson/800 AP/442 | |
---|---|---|---|
elongation | 断裂 | ASTM D412 | 500 % |
compression set | ASTM D395B | 24 % | |
Shore hardness | 邵氏 A | ASTM D2240 | 80 |
ASTM D2632 | 36 % | ||
Post curing time | 4.0 hr | ||
tensile strength | 屈服 | ASTM D412 | 38.6 MPa |
stripping time | 30 min |
Mechanical properties | Test Condition | Test Method | USA Anderson/800 AP/442 |
---|---|---|---|
tensile strength | 100%应变 | ASTM D412 | 4.14 MPa |
physical property | Test Condition | Test Method | USA Anderson/800 AP/442 |
---|---|---|---|
density | ASTM D1505 | 1.20 g/cm³ |