Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| optical property | Test Condition | Test Method | TORAY JAPAN/910X01 BK |
|---|---|---|---|
| transmissivity | 2000μm | Internal Method | 87.0 % |
| turbidity | 2000μm | Internal Method | 2.6 % |
| mechanical properties | Test Condition | Test Method | TORAY JAPAN/910X01 BK |
| Charpy Notched Impact Strength | 23℃ | ISO 179/1eA | 6.0 KJ/m22 |
| Tensile strain | 23℃,Break | ISO 527-2 | 13 % |
| Pencil hardness | 1kgf | JIS K5400 | H |
| bending strength | 23℃ | ISO 178 | 85.0 Mpa |
| Tensile stress | 23℃ | ISO 527-2 | 57.0 Mpa |
| Bending modulus | 23℃ | ISO 178 | 2430 Mpa |
| thermal performance | Test Condition | Test Method | TORAY JAPAN/910X01 BK |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 78.0 °C |
| UL flame retardant rating | UL 94 | HB | |
| Physical properties | Test Condition | Test Method | TORAY JAPAN/910X01 BK |
| melt mass-flow rate | 220℃/10kg | ISO 1133 | 28 g/10min |