Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC GP2102-WA597 LG GUANGZHOU
LUPOY®
Electrical field,Electronic field
Glass fiber reinforced,Chemical resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | LG GUANGZHOU/GP2102-WA597 |
---|---|---|---|
Rockwell hardness | R-Scale, 23°C, Injection | ASTM D785 | 124 |
thermal performance | Test Condition | Test Method | LG GUANGZHOU/GP2102-WA597 |
---|---|---|---|
Hot deformation temperature | 1.8 MPa, Unannealed, 6.40 mm, Injection | ASTM D648 | 137 °C |
RTI | UL 746 | 80.0 °C | |
RTI Elec | UL 746 | 80.0 °C | |
RTI Imp | UL 746 | 80.0 °C |
mechanical properties | Test Condition | Test Method | LG GUANGZHOU/GP2102-WA597 |
---|---|---|---|
Bending modulus | 23°C, 3.20 mm, Injection | ASTM D790 | 3330 Mpa |
bending strength | 23°C, 3.20 mm, Injection | ASTM D790 | 98.1 Mpa |
elongation | Break, 23°C, 3.20 mm, Injection | ASTM D638 | 15 % |
tensile strength | Yield, 23°C, 3.20 mm, Injection | ASTM D638 | 53.9 Mpa |
Physical properties | Test Condition | Test Method | LG GUANGZHOU/GP2102-WA597 |
---|---|---|---|
density | ASTM D792 | 1.25 g/cm³ | |
melt mass-flow rate | 300°C/1.2 kg | ASTM D1238 | 9.0 g/10 min |
Shrinkage rate | 23°C, 3.20 mm, Injection,Flow | ASTM D955 | 0.20 - 0.40 % |
impact performance | Test Condition | Test Method | LG GUANGZHOU/GP2102-WA597 |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C, 3.20 mm, Injection | ASTM D256 | 270 J/m |
flammability | Test Condition | Test Method | LG GUANGZHOU/GP2102-WA597 |
---|---|---|---|
UL flame retardant rating | 0.75 mm | UL 94 | HB |
injection | Test Condition | Test Method | LG GUANGZHOU/GP2102-WA597 |
---|---|---|---|
Back pressure | 0.981 to 3.92 Mpa | ||
drying temperature | 100 to 120 °C | ||
drying time | 3.0 to 5.0 hr | ||
Minimum Moisture Content | 0.020 % | ||
Mold temperature | 90 to 110 °C | ||
Processing (melt) temperature | 295 to 310 °C | ||
Screw speed | 40 to 70 rpm | ||
Spray nozzle temperature | 290 to 305 °C | ||
Suggested maximum moisture content | 0.020 % | ||
Temperature at the front of the material cylinder | 290 to 305 °C | ||
Temperature at the rear of the barrel | 280 to 295 °C | ||