Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PC VRY2200 UNIGEL BRAZIL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodUNIGEL BRAZIL/VRY2200
Impact strength of cantilever beam gap3.20mmASTM D256830 J/m
hardnessTest ConditionTest MethodUNIGEL BRAZIL/VRY2200
Rockwell hardnessM级ASTM D78575
R级ASTM D785120
Mechanical propertiesTest ConditionTest MethodUNIGEL BRAZIL/VRY2200
Flexural modulusASTMD7902350 MPa
elongation断裂ASTMD638100 %
Tensile modulusASTMD6382300 MPa
tensile strength 断裂ASTMD63873.0 MPa
屈服ASTMD63868.0 MPa
bending strengthASTMD79095.0 MPa
Electrical performanceTest ConditionTest MethodUNIGEL BRAZIL/VRY2200
Dissipation Factor60HzASTM D1506.6E-04
dielectric constant60HzASTM D1502.91
Volume resistivityASTM D2571E+16 ohms·cm
Dissipation Factor1MHzASTM D1509.2E-03
dielectric constant1MHzASTM D1502.85
dielectric strength1.60mmASTM D14929 kV/mm
arc resistanceASTM D495110 sec
optical performance Test ConditionTest MethodUNIGEL BRAZIL/VRY2200
refractive indexASTMD5421.586
transmissivityASTM D100389.0 %
flammabilityTest ConditionTest MethodUNIGEL BRAZIL/VRY2200
UL flame retardant rating3.0mmUL 94V-0
Hot filament ignition temperature3.2mmIEC 60695-2-13960 °C
physical property Test ConditionTest MethodUNIGEL BRAZIL/VRY2200
Shrinkage rateMDASTM D9550.50to0.70 %
densityASTMD7921.20 g/cm³
melt mass-flow rate300°C/1.2kgASTMD123812 g/10min
Water absorption rate23°C,24hrASTM D5700.23 %
Thermal performanceTest ConditionTest MethodUNIGEL BRAZIL/VRY2200
Heat distortion temperature1.8MPa,未退火,HDTASTMD648132 °C
Linear coefficient of thermal expansionMDASTM D6966.5E-05 cm/cm/°C

Contact Us

Get App

Top