Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PBT 7407 JAPAN POLYPLASTIC
DURANEX®
Electronic and electrical components,Automotive Applications
Glass fiber reinforced,Filler: Glass fiber glass,40% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | JAPAN POLYPLASTIC/7407 |
|---|---|---|---|
| Rockwell hardness | M-Scale | ISO 2039-2 | 85 |
| Supplementary Information | Test Condition | Test Method | JAPAN POLYPLASTIC/7407 |
|---|---|---|---|
| ColourNumber | EF2001/ED3002 |
| thermal performance | Test Condition | Test Method | JAPAN POLYPLASTIC/7407 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 200 °C |
| Linear coefficient of thermal expansion | MD:23to55°C | Internal Method | 2E-05 cm/cm/°C |
| TD:23to55°C | Internal Method | 5E-05 cm/cm/°C |
| mechanical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/7407 |
|---|---|---|---|
| Bending modulus | ISO 178 | 9500 Mpa | |
| bending strength | ISO 178 | 180 Mpa | |
| Tensile strain | Break | ISO 527-2 | 2.5 % |
| tensile strength | ISO 527-2 | 117 Mpa |
| Electrical performance | Test Condition | Test Method | JAPAN POLYPLASTIC/7407 |
|---|---|---|---|
| Compared to the anti leakage trace index | IEC 60112 | PLC 2 | |
| Dielectric strength | 3.00mm | IEC 60243-1 | 26 KV/mm |
| Volume resistivity | IEC 60093 | 3E+15 ohms·cm |
| Physical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/7407 |
|---|---|---|---|
| density | ISO 1183 | 1.57 g/cm³ | |
| Water absorption rate | 23°C,24hr | ISO 62 | 0.10 % |
| impact performance | Test Condition | Test Method | JAPAN POLYPLASTIC/7407 |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 8.8 kJ/m² |
| flammability | Test Condition | Test Method | JAPAN POLYPLASTIC/7407 |
|---|---|---|---|
| UL flame retardant rating | UL 94 | HB |