| impact performance | Test Condition | Test Method | BOREALIS EUROPE/BE860MO |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 8.0 kJ/m² |
| Multi axis Instrumented Impact Energy | 0°C,TotalPenetrationEnergy | ISO 6603-2 | 35.0 J |
| Charpy Notched Impact Strength | -20°C | ISO 179/1eA | 4.0 kJ/m² |
| Multi axis Instrumented Impact Energy | -20°C,TotalPenetrationEnergy | ISO 6603-2 | 25.0 J |
| Physical properties | Test Condition | Test Method | BOREALIS EUROPE/BE860MO |
| density | ISO 1183 | 0.902 g/cm³ | |
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 13 g/10min |
| Shrinkage rate | 1.0-2.0 % | ||
| mechanical properties | Test Condition | Test Method | BOREALIS EUROPE/BE860MO |
| tensile strength | Yield,Injection | ISO 527-2/50 | 25.0 Mpa |
| Tensile modulus | Injection | ISO 527-2/1 | 1250 Mpa |
| Tensile strain | Yield,Injection | ISO 527-2/50 | 6.0 % |
| thermal performance | Test Condition | Test Method | BOREALIS EUROPE/BE860MO |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 85.0 °C |
| hardness | Test Condition | Test Method | BOREALIS EUROPE/BE860MO |
| Rockwell hardness | R-Scale | ISO 2039-2 | 86 |