Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| mechanical properties | Test Condition | Test Method | COVESTRO GERMANY/DP.9365D |
|---|---|---|---|
| tensile strength | 10% Strain, 23°C | DIN 53504 | 20.0 Mpa |
| Tensile strain | Break, 23°C | DIN 53504 | 340 % |
| tensile strength | 300% Strain, 23°C | DIN 53504 | 50.0 Mpa |
| Bending modulus | 23°C | ISO 178 | 335 Mpa |
| tensile strength | Break, 23°C | DIN 53504 | 58.0 Mpa |
| 100% Strain, 23°C | DIN 53504 | 30.0 Mpa | |
| 50% Strain, 23°C | DIN 53504 | 26.0 Mpa | |
| injection | Test Condition | Test Method | COVESTRO GERMANY/DP.9365D |
| Mold temperature | 60 °C | ||
| drying temperature | < 110 °C | ||
| Processing (melt) temperature | 230 to 240 °C | ||
| squeeze out | Test Condition | Test Method | COVESTRO GERMANY/DP.9365D |
| Melt Temperature | 210 to 240 °C | ||
| drying temperature | < 110 °C | ||
| hardness | Test Condition | Test Method | COVESTRO GERMANY/DP.9365D |
| Shore hardness | Shore D, 1 Sec, 23°C | ISO 7619 | 66 |