injectionTest ConditionTest MethodCELANESE USA/UV140LG CG35131
Back pressure< 4.00 Mpa
Injection speed
Temperature in the middle of the barrel170 to 180 °C
Temperature at the front of the material cylinder175 to 185 °C
Spray nozzle temperature185 to 195 °C
Mold temperature80 to 105 °C
drying temperature100 to 120 °C
Processing (melt) temperature180 to 195 °C
drying time3.0 to 4.0 hr
Temperature at the rear of the barrel170 to 175 °C
mechanical propertiesTest ConditionTest MethodCELANESE USA/UV140LG CG35131
tensile strengthYieldISO 527-2/1A/5048.0 Mpa
Tensile modulusISO 527-2/1A2100 Mpa
Tensile strainYieldISO 527-2/1A/5010 %
thermal performanceTest ConditionTest MethodCELANESE USA/UV140LG CG35131
Hot deformation temperature1.8 MPa, UnannealedISO 75-2/A85.0 °C
Melting temperatureISO 11357-3168 °C
Physical propertiesTest ConditionTest MethodCELANESE USA/UV140LG CG35131
Shrinkage rateFlowISO 294-42.0 %
横向FlowISO 294-41.8 %
Melt Volume Flow Rate (MVR)190°C/2.16 kgISO 113313.0 cm3/10min