Unspecified TATREN® TPO 20 77 SLOVAK SLOVNAFT
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodSLOVAK SLOVNAFT/TATREN® TPO 20 77
Impact strength of cantilever beam gap-20°C,注塑ISO 180/A30 kJ/m²
-30°C,注塑ISO 180/A>10 kJ/m²
23°C,注塑ISO 180/A42 kJ/m²
Mechanical propertiesTest ConditionTest MethodSLOVAK SLOVNAFT/TATREN® TPO 20 77
Flexural modulus注塑ISO 178950 MPa
tensile strength 屈服,注塑ISO 527-219.0 MPa
Tensile modulus注塑ISO 527-21050 MPa
Tensile strain屈服,注塑ISO 527-210 %
physical property Test ConditionTest MethodSLOVAK SLOVNAFT/TATREN® TPO 20 77
melt mass-flow rate230°C/2.16kgISO 113320 g/10min
Thermal performanceTest ConditionTest MethodSLOVAK SLOVNAFT/TATREN® TPO 20 77
Heat distortion temperature0.45MPa,未退火,HDTISO 75-2/B81.0 °C