Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
HDPE HC 7260 PETROCHINA JILIN
--
--
high density、High hardness、High stiffness、Low warpage
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Basic performanceTest ConditionTest MethodPETROCHINA JILIN/HC 7260
melt mass-flow rate190℃/2.16kgASTM D-12388 g/10min
densityASTM D-7920.959 g/cm
Mechanical propertiesTest ConditionTest MethodPETROCHINA JILIN/HC 7260
tensile strength 屈服,Compression MoldedASTM D-63829 Mpa
elongation at yieldCompression MoldedASTM D-6387.5 %
Shore hardnessShore D,15 sec,Compression MoldedASTM D-224063
Flexural modulusCompression Molded,2% SecantASTM D-7901140 Mpa
Impact strength of cantilever beam gapCompression MoldedASTM D-25635 J/m
Environmental stress cracking resistance50℃,2mm,100% Igepal,Compression Molded,F50ASTM D-1693B5 hr
Thermal performanceTest ConditionTest MethodPETROCHINA JILIN/HC 7260
vicatASTM D-1525126 °C
Heat distortion temperature0.45MPa, Unannealed,Compression Molded,HDTASTM D-64876 °C

Contact Us

Get App

Top