PPS A604X95-NC TORAY JAPAN
Torelina®
Electrical components
High mobility,Low burr edge,Filler: Glass fiber reinf,40% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | TORAY JAPAN/A604X95-NC |
|---|---|---|---|
| Rockwell hardness | R-Scale | ISO 2039-2 | 122 |
| Supplementary Information | Test Condition | Test Method | TORAY JAPAN/A604X95-NC |
|---|---|---|---|
| BarFlowLength | 320°C,1.00mm | Internal Method | 165 mm |
| thermal performance | Test Condition | Test Method | TORAY JAPAN/A604X95-NC |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 260 °C |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 3.5E-05 cm/cm/°C |
| MD | ISO 11359-2 | 2.3E-05 cm/cm/°C | |
| Melting temperature | ISO 11357-3 | 278 °C |
| mechanical properties | Test Condition | Test Method | TORAY JAPAN/A604X95-NC |
|---|---|---|---|
| Bending modulus | 23°C | ISO 178 | 15000 Mpa |
| bending strength | 23°C | ISO 178 | 290 Mpa |
| Friction coefficient | 0.25 | ||
| shear strength | 23°C | JISK7214 | 75.0 Mpa |
| Taber abraser | 1000Cycles | ISO 9352 | 50.0 mg |
| Tensile strain | Break,23°C | ISO 527-2 | 1.7 % |
| tensile strength | Yield,23°C | ISO 527-2 | 190 Mpa |
| Electrical performance | Test Condition | Test Method | TORAY JAPAN/A604X95-NC |
|---|---|---|---|
| Dielectric constant | 23°C,1MHz | IEC 60250 | 3.60 |
| Dielectric strength | IEC 60243-1 | 25 KV/mm | |
| Dissipation factor | 23°C,1MHz | IEC 60250 | 2E-03 |
| Volume resistivity | IEC 60093 | 1E+16 ohms·cm |
| Physical properties | Test Condition | Test Method | TORAY JAPAN/A604X95-NC |
|---|---|---|---|
| Shrinkage rate | TD:3.00mm2 | Internal Method | 0.80 % |
| MD:3.00mm4 | Internal Method | 0.20 % | |
| Water absorption rate | 23°C,24hr | ISO 62 | 0.020 % |
| impact performance | Test Condition | Test Method | TORAY JAPAN/A604X95-NC |
|---|---|---|---|
| Impact strength of simply supported beam without notch | 23°C | ISO 179 | 45 kJ/m² |
| flammability | Test Condition | Test Method | TORAY JAPAN/A604X95-NC |
|---|---|---|---|
| UL flame retardant rating | 0.200mm | UL 94 | V-0 |