Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| Other performance | Test Condition | Test Method | SINOPEC MAOMING/PPR-MT18S |
|---|---|---|---|
| turbidity | GB/T 2410-2008 | 12.4 % | |
| mechanical properties | Test Condition | Test Method | SINOPEC MAOMING/PPR-MT18S |
| Tensile stress | Q/SH PRD255-2009(2012) | 32.7 Mpa | |
| Bending modulus | Q/SH PRD255-2009(2012) | 1294 Mpa | |
| Charpy Notched Impact Strength | 23℃ | Q/SH PRD255-2009(2012) | 2.0 kJ/m² |
| Electrical performance | Test Condition | Test Method | SINOPEC MAOMING/PPR-MT18S |
| ash content | 质量分数 | Q/SH PRD255-2009(2012) | 0.015 % |
| thermal performance | Test Condition | Test Method | SINOPEC MAOMING/PPR-MT18S |
| Hot deformation temperature | Tf0.45 | Q/SH PRD255-2009(2012) | 77.7 °C |
| Physical properties | Test Condition | Test Method | SINOPEC MAOMING/PPR-MT18S |
| melt mass-flow rate | Q/SHPRD255-2009(2012) | 19.8 g/10min |