| thermal performance | Test Condition | Test Method | TAIWAN GINAR/A0520FN B2 |
|---|---|---|---|
| Melting temperature | ASTM D789 | 260 °C | |
| Hot deformation temperature | 1.8 MPa, Unannealed | ASTM D648 | 235 °C |
| UL flame retardant rating | 0.0313 mm | UL 94 | V-0 |
| mechanical properties | Test Condition | Test Method | TAIWAN GINAR/A0520FN B2 |
| elongation | Break | ASTM D638 | 2.5 % |
| Impact strength of cantilever beam gap | 23℃ | ASTM D256 | 77 J/m |
| Rockwell hardness | R -Sale | ASTM D785 | 120 |
| bending strength | ASTM D790 | 193 Mpa | |
| tensile strength | Yield | ASTM D638 | 131 Mpa |
| Bending modulus | ASTM D790 | 8270 Mpa | |
| Physical properties | Test Condition | Test Method | TAIWAN GINAR/A0520FN B2 |
| Water absorption rate | 23℃, 24 hr | ASTM D570 | 0.80 % |
| Shrinkage rate | Flow:3.00 mm | ASTM D955 | 0.50 % |