Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP G2 U02 LYONDELLBASELL HOLAND
Moplen
Automotive sector,Engine hood parts,Electrical appliances
Glass fiber reinforced,Chemical coupling,High rigidity,High mobility,Anti creep
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | LYONDELLBASELL HOLAND/G2 U02 |
---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 130 °C |
Vicat softening temperature | ISO 306/B | 125 °C |
mechanical properties | Test Condition | Test Method | LYONDELLBASELL HOLAND/G2 U02 |
---|---|---|---|
Tensile modulus | 23°C | ISO 527-2 | 4600 Mpa |
Tensile strain | Break | ISO 527-2 | 4.0 % |
tensile strength | Break,23°C | ISO 527-2 | 70.0 Mpa |
Physical properties | Test Condition | Test Method | LYONDELLBASELL HOLAND/G2 U02 |
---|---|---|---|
melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 14 g/10min |
Melt Volume Flow Rate (MVR) | 230°C/2.16kg | ISO 1133 | 17.0 cm3/10min |
impact performance | Test Condition | Test Method | LYONDELLBASELL HOLAND/G2 U02 |
---|---|---|---|
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 40 kJ/m² |