POM H2320-004 BASF KOREA
Ultraform®
Thick walled components
high molecular weight、Ultral&reg
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Mechanical properties | Test Condition | Test Method | BASF KOREA/H2320-004 |
---|---|---|---|
Tensile creep modulus | 1000h | ISO 899-1 | 189000 psi |
Tensile stress | 73℉ | ISO 527-1 | 9280 psi |
Tensile strain | 73℉,屈服 | ISO 527-1 | 11 % |
Charpy Notched Impact Strength | -22℉ | ISO 179 | 2.62 ft·lb/in |
Impact strength of simply supported beam without notch | -22℉ | ISO 179 | 99.9 ft·lb/in |
73℉ | ISO 179 | 119 ft·lb/in | |
Tensile modulus | 73℉ | ISO 527-1 | 377000 psi |
Charpy Notched Impact Strength | 73℉ | ISO 179 | 2.86 ft·lb/in |
Electrical performance | Test Condition | Test Method | BASF KOREA/H2320-004 |
---|---|---|---|
Dielectric loss | 1E+6HZ,73℉ | IEC 60250 | 0.00500 |
Volume resistivity | IEC 60093 | 1E+15 ohm·cm | |
IEC 60093 | 1E+13 ohms |
processability | Test Condition | Test Method | BASF KOREA/H2320-004 |
---|---|---|---|
process temperature | 374-446 ℉ |
physical property | Test Condition | Test Method | BASF KOREA/H2320-004 |
---|---|---|---|
Water absorption rate | 23C/50RH | ISO 62 | 0.2 % |
Thermal performance | Test Condition | Test Method | BASF KOREA/H2320-004 |
---|---|---|---|
Heat distortion temperature | 1.80MPa,HDT | ISO 75A-1 | 203 ℉ |
UL flame retardant rating | UL 94 | HB |