Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PCTG EX501 EASTMAN USA
Tritan™
Household daily necessiti、Electrical applications
Easy to process、heat-resisting
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | EASTMAN USA/EX501 |
---|---|---|---|
Suspended wall beam without notch impact strength | -40°C | ASTM D4812 | 无断裂 |
Dart impact | 内部方法 | No Crazes/No Impact Failures | |
23°C, Energy at Max Load | ASTM D3763 | 57.0 J | |
Suspended wall beam without notch impact strength | 23°C | ASTM D4812 | 无断裂 |
Dart impact | -40°C, Energy at Max Load | ASTM D3763 | 66.0 J |
hardness | Test Condition | Test Method | EASTMAN USA/EX501 |
---|---|---|---|
Rockwell hardness | R 级, 23°C | ASTM D785 | 109 |
Mechanical properties | Test Condition | Test Method | EASTMAN USA/EX501 |
---|---|---|---|
tensile strength | 断裂, 23°C | ISO 527-2 | 55.0 Mpa |
bending strength | 屈服, 23°C | ASTM D790 | 72.0 Mpa |
tensile strength | 屈服, 23°C | ASTM D638 | 45.0 Mpa |
elongation | 断裂, 23°C | ISO 527-2 | 150 % |
tensile strength | 屈服, 23°C | ISO 527-2 | 44.0 Mpa |
elongation | 断裂, 23°C | ASTM D638 | 180 % |
Tensile modulus | 23°C | ASTM D638 | 1520 Mpa |
23°C | ISO 527-2 | 1540 Mpa | |
elongation | 屈服, 23°C | ASTM D638 | 6.0 % |
tensile strength | 断裂, 23°C | ASTM D638 | 56.0 Mpa |
optical performance | Test Condition | Test Method | EASTMAN USA/EX501 |
---|---|---|---|
Shrinkage rate | Dishwasher | 内部方法 | 0.0 % |
transmissivity | 总计 | ASTM D1003 | 91.0 % |
Haze ratio | -- | ASTM D1003 | < 1.0 % |
Shrinkage rate | Boiling, 2 hr | 内部方法 | 2.3 % |
Boiling, 1 hr | 内部方法 | 1.9 % | |
Haze ratio | --3 | 内部方法 | < 6.0 % |
physical property | Test Condition | Test Method | EASTMAN USA/EX501 |
---|---|---|---|
Shrinkage rate | 注塑,Flow | ASTM D955 | 0.50 - 0.70 % |
Thermal performance | Test Condition | Test Method | EASTMAN USA/EX501 |
---|---|---|---|
Heat distortion temperature | 0.45 MPa, 未退火,HDT | ASTM D648 | 101 °C |
1.8 MPa, 未退火,HDT | ASTM D648 | 88.0 °C |
injection | Test Condition | Test Method | EASTMAN USA/EX501 |
---|---|---|---|
drying time | 4.0 to 6.0 hr | ||
Processing (melt) temperature | 260 to 282 °C | ||
drying temperature | 88 °C | ||
Temperature | 38 to 66 °C |