Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC 144R SABIC INNOVATIVE US
LEXAN™
Medical supplies,Nursing supplies,Non specific food
Flame retardant,transparent
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | SABIC INNOVATIVE US/144R |
|---|---|---|---|
| Rockwell hardness | M-Sale | ASTM D785 | 70 |
| R-Sale | ASTM D785 | 118 |
| thermal performance | Test Condition | Test Method | SABIC INNOVATIVE US/144R |
|---|---|---|---|
| Ball Pressure Test | 125°C | IEC 60695-10-2 | Pass |
| Hot deformation temperature | 1.8MPa,Unannealed,6.40mm | ASTM D648 | 132 °C |
| 0.45MPa,Unannealed,6.40mm | ASTM D648 | 137 °C | |
| 0.45MPa,Unannealed,100mmSpan | ISO 75-2/Be | 136 °C | |
| 1.8MPa,Unannealed,100mmSpan | ISO 75-2/Ae | 125 °C | |
| Linear coefficient of thermal expansion | MD:-40to95°C | ASTME831 | 6.8E-05 cm/cm/°C |
| MD:23to80°C | ISO 11359-2 | 7E-05 cm/cm/°C | |
| RTI Elec | UL 746 | 130 °C | |
| RTI Imp | UL 746 | 130 °C | |
| RTI Str | UL 746 | 130 °C | |
| specific heat | ASTMC351 | 1250 J/kg/°C | |
| thermal conductivity | ASTMC177 | 0.19 W/m/K | |
| ISO 8302 | 0.20 W/m/K | ||
| Vicat softening temperature | -- | ISO 306/B120 | 142 °C |
| -- | ISO 306/B50 | 141 °C | |
| ASTM D152510 | 154 °C | ||
| -- | ISO 306/A50 | 153 °C |
| mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE US/144R |
|---|---|---|---|
| Bending modulus | 50.0mmSpan | ASTM D790 | 2340 Mpa |
| ISO 178 | 2300 Mpa | ||
| bending strength | Yield,50.0mmSpan | ASTM D790 | 97.0 Mpa |
| ISO 178 | 90.0 Mpa | ||
| elongation | Break | ASTM D638 | 130 % |
| Yield | ASTM D638 | 7.0 % | |
| Taber abraser | 1000Cycles,1000g,CS-17Wheel | ASTM D1044 | 10.0 mg |
| Tensile modulus | ASTM D638 | 2370 Mpa | |
| ISO 527-2/1 | 2350 Mpa | ||
| Tensile strain | Break | ISO 527-2/50 | 110 % |
| Yield | ISO 527-2/50 | 6.0 % | |
| tensile strength | Yield | ASTM D638 | 62.0 Mpa |
| Yield | ISO 527-2/50 | 63.0 Mpa | |
| Break | ISO 527-2/50 | 70.0 Mpa | |
| Break | ASTM D638 | 68.0 Mpa |
| Electrical performance | Test Condition | Test Method | SABIC INNOVATIVE US/144R |
|---|---|---|---|
| Compared to the anti leakage trace index | CTI | UL 746 | PLC 2 |
| Dielectric constant | 1MHz | ASTM D150 | 2.96 |
| 50Hz | ASTM D150 | 3.17 | |
| 60Hz | ASTM D150 | 3.17 | |
| Dielectric strength | 3.20mm,in Oil | IEC 60243-1 | 17 KV/mm |
| 3.20mm,inAir | ASTM D149 | 15 KV/mm | |
| Dissipation factor | 1MHz | IEC 60250 | 0.010 |
| 50Hz | IEC 60250 | 1E-03 | |
| 1MHz | ASTM D150 | 0.010 | |
| 60Hz | ASTM D150 | 9E-04 | |
| 50Hz | ASTM D150 | 9E-04 | |
| 60Hz | IEC 60250 | 1E-03 | |
| High arc combustion index | HAI | UL 746 | PLC 1 |
| High voltage arc tracing rate | HVTR | UL 746 | PLC 2 |
| Hot wire ignition | HWI | UL 746 | PLC 2 |
| Relative permittivity | 60Hz | IEC 60250 | 2.70 |
| 50Hz | IEC 60250 | 2.70 | |
| 1MHz | IEC 60250 | 2.70 | |
| Surface resistivity | IEC 60093 | >1.0E+15 ohms | |
| Volume resistivity | ASTM D257 | >1.0E+17 ohms·cm | |
| IEC 60093 | >1.0E+15 ohms·cm |
| Physical properties | Test Condition | Test Method | SABIC INNOVATIVE US/144R |
|---|---|---|---|
| density | ASTM D792 | 1.20 g/cm³ | |
| melt mass-flow rate | 300°C/1.2kg | ASTM D1238 | 11 g/10min |
| Melt Volume Flow Rate (MVR) | 300°C/1.2kg | ISO 1133 | 10.0 cm3/10min |
| Shrinkage rate | MD:3.20mm | Internal Method | 0.50-0.70 % |
| Specific volume | ASTM D792 | 0.830 cm³/g | |
| Water absorption rate | Equilibrium,100°C | ASTM D570 | 0.58 % |
| 24hr | ASTM D570 | 0.15 % | |
| Equilibrium,23°C | ASTM D570 | 0.35 % |
| impact performance | Test Condition | Test Method | SABIC INNOVATIVE US/144R |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/2C | 35 kJ/m² |
| Dart impact | 23°C,EnergyatPeakLoad | ASTM D3763 | 63.0 J |
| 23°C | ASTM D3029 | 169 J | |
| Impact strength of cantilever beam gap | Natural,Tints | ASTM D256 | 800 J/m |
| -30°C | ISO 180/1A | 10 kJ/m² | |
| 23°C | ISO 180/1A | 12 kJ/m² | |
| 23°C | ASTM D256 | 800 J/m | |
| 23°C | ASTM D4812 | 3200 J/m | |
| Colors | ASTM D256 | 800 J/m | |
| ASTM D1822 | 577 kJ/m² |
| flammability | Test Condition | Test Method | SABIC INNOVATIVE US/144R |
|---|---|---|---|
| Extreme Oxygen Index | ASTM D2863 | 25 % | |
| ISO 4589-2 | 25 % | ||
| UL flame retardant rating | 1.5mm | UL 94 | HB |
| optical performance | Test Condition | Test Method | SABIC INNOVATIVE US/144R |
|---|---|---|---|
| Refractive index | ASTM D542 | 1.586 | |
| transmissivity | 2540μm | ASTM D1003 | 88.0 % |
| turbidity | 2540μm | ASTM D1003 | 1.0 % |