Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 6M30 DOMO CHEM GERMANY
--
--
Mineral reinforcement,filler,Mineral filler,30%,Filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | DOMO CHEM GERMANY/6M30 |
---|---|---|---|
Rockwell hardness | R-Scale | ISO 2039-2 | 115 |
thermal performance | Test Condition | Test Method | DOMO CHEM GERMANY/6M30 |
---|---|---|---|
Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 185 °C |
1.8MPa,Unannealed | ISO 75-2/A | 90.0 °C | |
Melting temperature | ISO 11357-3 | 218to222 °C | |
Vicat softening temperature | ISO 306/B50 | 200 °C |
mechanical properties | Test Condition | Test Method | DOMO CHEM GERMANY/6M30 |
---|---|---|---|
Tensile modulus | ISO 527-2/1 | 4800 Mpa | |
Tensile strain | Break | ISO 527-2/5 | 12 % |
tensile strength | Break | ISO 527-2/5 | 85.0 Mpa |
Electrical performance | Test Condition | Test Method | DOMO CHEM GERMANY/6M30 |
---|---|---|---|
Surface resistivity | IEC 60093 | 1E+13 ohms | |
Volume resistivity | IEC 60093 | 1E+15 ohms·cm |
Physical properties | Test Condition | Test Method | DOMO CHEM GERMANY/6M30 |
---|---|---|---|
density | ISO 1183 | 1.36 g/cm³ | |
Shrinkage rate | MD2:23°C,72hr | ISO 2577 | 0.90-1.1 % |
impact performance | Test Condition | Test Method | DOMO CHEM GERMANY/6M30 |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 4.5 kJ/m² |
flammability | Test Condition | Test Method | DOMO CHEM GERMANY/6M30 |
---|---|---|---|
Burning rate | FMVSS302 | <100 mm/min | |
UL flame retardant rating | 0.8mm | UL 94 | HB |