PA+PPO(PPE) Infino HC-8040 LOTTE KOREA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | LOTTE KOREA/Infino HC-8040 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 20 kJ/m² |
Impact strength of cantilever beam gap | 23°C,6.35mm | ASTM D256 | 180 J/m |
23°C5 | ISO 180/1A | 20 kJ/m² | |
23°C,3.18mm | ASTM D256 | 200 J/m |
hardness | Test Condition | Test Method | LOTTE KOREA/Infino HC-8040 |
---|---|---|---|
Rockwell hardness | R计秤 | ISO 2039-2 | 114 |
R级 | ASTM D785 | 114 |
Mechanical properties | Test Condition | Test Method | LOTTE KOREA/Infino HC-8040 |
---|---|---|---|
tensile strength | 屈服2 | ASTM D638 | 60.0 MPa |
bending strength | --3 | ASTM D790 | 84.0 MPa |
elongation | 断裂2 | ASTM D638 | 30 % |
断裂 | ISO 527-2/50 | 27 % | |
Flexural modulus | --3 | ASTM D790 | 2200 MPa |
--4 | ISO 178 | 2100 MPa | |
Tensile modulus | -- | ISO 527-2/20 | 2100 MPa |
bending strength | --4 | ISO 178 | 94.0 MPa |
tensile strength | 屈服 | ISO 527-2/50 | 60.0 MPa |
Tensile modulus | --2 | ASTM D638 | 2000 MPa |
tensile strength | 断裂2 | ASTM D638 | 60.0 MPa |
断裂 | ISO 527-2/50 | 60.0 MPa |
physical property | Test Condition | Test Method | LOTTE KOREA/Infino HC-8040 |
---|---|---|---|
Shrinkage rate | MD:3.20mm | ASTM D955 | 0.90to1.2 % |
density | ASTMD792 | 1.10 g/cm³ | |
Shrinkage rate | TD:3.20mm | ISO 2577 | 0.90to1.1 % |
TD:3.20mm | ASTM D955 | 0.90to1.1 % | |
melt mass-flow rate | 280°C/5.0kg | ASTMD1238 | 22 g/10min |
Shrinkage rate | MD:3.20mm | ISO 2577 | 0.90to1.2 % |
Thermal performance | Test Condition | Test Method | LOTTE KOREA/Infino HC-8040 |
---|---|---|---|
Linear coefficient of thermal expansion | MD:40到100°C | ASTME831 | 9E-05 cm/cm/°C |
Heat distortion temperature | 1.8MPa,未退火,6.40mm,HDT | ASTM D648 | 108 °C |
Linear coefficient of thermal expansion | TD:40到100°C | ASTME831 | 1.1E-04 cm/cm/°C |
TD:-40到40°C | ASTME831 | 8.5E-05 cm/cm/°C | |
Heat distortion temperature | 1.8MPa,未退火,4.00mm,HDT | ISO 75-2/A | 85.0 °C |
Linear coefficient of thermal expansion | MD:-40到40°C | ASTME831 | 8E-05 cm/cm/°C |