Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

AES HW600FR KUMHO KOREA
--
Electrical/Electronic App、currency、Outdoor applications
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Mechanical properties | Test Condition | Test Method | KUMHO KOREA/HW600FR |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | ASTM D256 | 182 J/m |
bending strength | 23°C | ASTM D790 | 55 Mpa |
elongation at break | 23°C | ASTM D638 | 15 % |
Flexural modulus | 23°C | ASTM D790 | 2000 Mpa |
tensile strength | 23°C | ASTM D638 | 40 Mpa |
Flame retardant performance | Test Condition | Test Method | KUMHO KOREA/HW600FR |
---|---|---|---|
UL flame retardant rating | UL -94 | V-0 - |
physical property | Test Condition | Test Method | KUMHO KOREA/HW600FR |
---|---|---|---|
melt mass-flow rate | 220℃/10Kg | ASTM D1238 | 6.0 g/10min |
Shrinkage rate | MD | ASTM D995 | 0.30 % |
TD | ASTM D995 | 0.60 % |
Thermal performance | Test Condition | Test Method | KUMHO KOREA/HW600FR |
---|---|---|---|
vicat | ASTM1525 | 86 °C | |
Heat distortion temperature | 1.80MPa未退火,HDT | ASTM D648 | 80 °C |