PVC SMOKEGUARD™ III 1041 NATURAL Alphagary
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | Alphagary/SMOKEGUARD™ III 1041 NATURAL |
---|---|---|---|
Shore hardness | 邵氏D | ASTM D2240 | 67to73 |
邵氏D,15秒 | ASTM D2240 | 54to60 |
Electrical performance | Test Condition | Test Method | Alphagary/SMOKEGUARD™ III 1041 NATURAL |
---|---|---|---|
dielectric constant | 23°C,100MHz | ASTM D150 | 3.35 |
Dissipation Factor | 23°C,100MHz | ASTM D150 | 0.014 |
flammability | Test Condition | Test Method | Alphagary/SMOKEGUARD™ III 1041 NATURAL |
---|---|---|---|
Limiting Oxygen Index | 3.18mm | ASTM D2863 | 51 % |
physical property | Test Condition | Test Method | Alphagary/SMOKEGUARD™ III 1041 NATURAL |
---|---|---|---|
density | ASTM D792 | 1.57to1.61 g/cm³ |
aging | Test Condition | Test Method | Alphagary/SMOKEGUARD™ III 1041 NATURAL |
---|---|---|---|
elongation at break | 100°C,240hr | UL Unspecified | -7.0 % |
Change rate of tensile strength in air | 100°C,240hr | UL Unspecified | -1.0 % |
elastomer | Test Condition | Test Method | Alphagary/SMOKEGUARD™ III 1041 NATURAL |
---|---|---|---|
tensile strength | 0.381mm | ASTM D412 | 17.9 MPa |
elongation | Break,1.91mm | ASTM D412 | 210 % |
tensile strength | 1.91mm | ASTM D412 | 15.9 MPa |
elongation | Break,0.381mm | ASTM D412 | 190 % |
Thermal performance | Test Condition | Test Method | Alphagary/SMOKEGUARD™ III 1041 NATURAL |
---|---|---|---|
brittle temperature | ASTM D746 | -4.00 °C |