Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP J800R HYOSUNG KOREA
TOPILENE®
Household goods、Electrical appliances、Industrial applications
--
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | HYOSUNG KOREA/J800R |
---|---|---|---|
Impact strength of cantilever beam gap | -10°C | ASTMD256 | 39 J/m |
23°C | ASTMD256 | 78 J/m |
Mechanical properties | Test Condition | Test Method | HYOSUNG KOREA/J800R |
---|---|---|---|
Flexural modulus | ASTMD790 | 1720 Mpa |
physical property | Test Condition | Test Method | HYOSUNG KOREA/J800R |
---|---|---|---|
melt mass-flow rate | 230°C/2.16kg | ASTMD1238 | 18 g/10min |
Contact Us
Get App
Top