PC AG1760 IDEMITSU JAPAN
TARFLON NEO™
Automotive Applications、Electronic and electrical
High mobility、Medium viscosity
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | IDEMITSU JAPAN/AG1760 |
---|---|---|---|
Rockwell hardness | R计秤 | ISO 2039-2 | 120 |
M计秤 | ISO 2039-2 | 40 |
Supplementary Information | Test Condition | Test Method | IDEMITSU JAPAN/AG1760 |
---|---|---|---|
ISO Shortcut | >PC< |
Mechanical properties | Test Condition | Test Method | IDEMITSU JAPAN/AG1760 |
---|---|---|---|
Nominal tensile fracture strain | ISO 527-2 | 100 % | |
bending strength | ISO 178 | 90.0 Mpa | |
Flexural modulus | ISO 178 | 2100 Mpa | |
tensile strength | 屈服 | ISO 527-2 | 55.0 Mpa |
flammability | Test Condition | Test Method | IDEMITSU JAPAN/AG1760 |
---|---|---|---|
UL flame retardant rating | 0.5-3.0mm | UL 94 | V-2 |
physical property | Test Condition | Test Method | IDEMITSU JAPAN/AG1760 |
---|---|---|---|
Shrinkage rate | TD:2.00mm | 内部方法 | 0.60-0.80 % |
spiral flow length | 内部方法 | 28.0 CM | |
Melt volume flow rate | 300°C/1.2kg | ISO 1133 | 13.0 cm3/10min |
Water absorption rate | 平衡,23°C,50%RH | ISO 62 | 0.20 % |
Shrinkage rate | MD:2.00mm | 内部方法 | 0.60-0.80 % |
Thermal performance | Test Condition | Test Method | IDEMITSU JAPAN/AG1760 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 122 °C |
Linear coefficient of thermal expansion | MD | ISO 11359-2 | 7E-05 cm/cm/°C |