Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC LPC1001F BK LUCK ENPLA KOREA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | LUCK ENPLA KOREA/LPC1001F BK |
---|---|---|---|
Hot deformation temperature | 1.8 MPa, Unannealed | ASTM D648 | 122 °C |
mechanical properties | Test Condition | Test Method | LUCK ENPLA KOREA/LPC1001F BK |
---|---|---|---|
Bending modulus | ASTM D790 | 2280 Mpa | |
bending strength | ASTM D790 | 82.4 Mpa | |
tensile strength | ASTM D638 | 53.0 Mpa |
Physical properties | Test Condition | Test Method | LUCK ENPLA KOREA/LPC1001F BK |
---|---|---|---|
melt mass-flow rate | 260°C/5.0 kg | ASTM D1238 | 22 g/10 min |
Shrinkage rate | Flow | ASTM D955 | 0.60 - 0.65 % |
impact performance | Test Condition | Test Method | LUCK ENPLA KOREA/LPC1001F BK |
---|---|---|---|
Suspended wall beam without notch impact strength | 3.18 mm | ASTM D256 | 590 J/m |
flammability | Test Condition | Test Method | LUCK ENPLA KOREA/LPC1001F BK |
---|---|---|---|
UL flame retardant rating | 0.8 mm | UL 94 | V-0 |
injection | Test Condition | Test Method | LUCK ENPLA KOREA/LPC1001F BK |
---|---|---|---|
Back pressure | 0.490 to 2.94 Mpa | ||
drying temperature | 100 to 110 °C | ||
drying time | 3.0 to 5.0 hr | ||
Mold temperature | 50 to 80 °C | ||
Screw speed | 30 to 50 rpm | ||
Spray nozzle temperature | 295 to 315 °C | ||
Temperature at the front of the material cylinder | 285 to 305 °C | ||
Temperature at the rear of the barrel | 270 to 290 °C | ||
Temperature in the middle of the barrel | 280 to 300 °C |