| mechanical properties | Test Condition | Test Method | UMG JAPAN/TR-2 |
|---|---|---|---|
| Charpy Notched Impact Strength | ASTM D256/ISO 179 | 18 kg·cm/cm(J/M)ft·lb/in | |
| melt mass-flow rate | 14 g/10min | ||
| Bending modulus | 2500 Mpa | ||
| ASTM D790/ISO 178 | 2.500 kg/cm²(MPa)[Lb/in²] | ||
| Charpy Notched Impact Strength | 18 kJ/m² | ||
| thermal performance | Test Condition | Test Method | UMG JAPAN/TR-2 |
| Hot deformation temperature | HDT | ASTM D648/ISO 75 | 83 ℃(℉) |
| UL flame retardant rating | UL 94 | HB | |
| Hot deformation temperature | HDT | 83 °C | |
| other | Test Condition | Test Method | UMG JAPAN/TR-2 |
| characteristic | 耐热 | ||
| Physical properties | Test Condition | Test Method | UMG JAPAN/TR-2 |
| melt mass-flow rate | ASTM D1238/ISO 1133 | 14 g/10min |