Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PC 301-15 SUMITOMO JAPAN
SD POLYCA™ 
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

thermal performanceTest ConditionTest MethodSUMITOMO JAPAN/301-15
Hot deformation temperature1.8 MPa1.80MPaISO 75/Af126 °C
Linear coefficient of thermal expansionMDMDISO 11359-20.000070 cm/cm/℃
TDTDISO 11359-20.000070 cm/cm/℃
mechanical propertiesTest ConditionTest MethodSUMITOMO JAPAN/301-15
Bending modulusISO 1782300 Mpa
bending strengthISO 17892 Mpa
Rockwell hardnessR-ScaleRISO 2039118
Tensile modulusISO 527-22300 Mpa
Tensile strainBreakBreakISO 527-2110 %
Tensile stressYieldISO 527-260 Mpa
flame retardant performanceTest ConditionTest MethodSUMITOMO JAPAN/301-15
UL flame retardant rating1.00 mmUL 94HB
0.75 mmUL 94V-2
3.00 mmUL 94HB
0.44 mmUL 94V-2
Electrical performanceTest ConditionTest MethodSUMITOMO JAPAN/301-15
Compared to the anti leakage trace indexIEC 60112 V
Dielectric strength1 mm1mmIEC 6024331 KV/mm
Dissipation factor1 MHz,2 mm1MHz, 2mmIEC 602500.09
2 mm,100 Hz100Hz, 2mmIEC 602500.001
Relative permittivity100 Hz,2 mm100Hz, 2mmIEC 602503
1 MHz,2mm1MHz, 2mmIEC 602503
Surface resistivityIEC 60093≧1.0E+15
Volume resistivityIEC 6009330000000000000000 ohms·cm
Physical propertiesTest ConditionTest MethodSUMITOMO JAPAN/301-15
densityISO 11831.2 g/cm³
melt mass-flow rate300℃,1.20kg300℃,1.2kgISO 113315 g/10min
Melt Volume Flow Rate (MVR)300℃,1.2 kg300℃,1.2kgISO 113314 cm3/10min
Shrinkage rateTDTDInternal Method0.5-0.7 %
MDMDInternal Method0.5-0.7 %
Water absorption rate23℃,24hr23℃,24hrsISO 620.2 %
impact performanceTest ConditionTest MethodSUMITOMO JAPAN/301-15
Charpy Notched Impact StrengthUnnotchedUnnotched,23℃,5mmISO 179-1NB kJ/m²
NotchedNotched,23℃,4mmISO 179-170 kJ/m²
optical performanceTest ConditionTest MethodSUMITOMO JAPAN/301-15
Refractive indexISO 4891.585
Total Light Transmittance2mm2mmISO 1346889 %
turbidity2 mm2mmISO 147820.4 %