| mechanical properties | Test Condition | Test Method | TEIJIN SINGAPORE/L-1225L |
|---|---|---|---|
| Tensile modulus | ASTM D638/ISO 527 | 2170 kg/cm²(MPa)[Lb/in²] | |
| Elongation at Break | ASTM D638/ISO 527 | 50 % | |
| Bending modulus | ASTM D790/ISO 178 | 2280 kg/cm²(MPa)[Lb/in²] | |
| bending strength | ASTM D790/ISO 178 | 90 kg/cm²(MPa)[Lb/in²] | |
| Rockwell hardness | ASTM D785 | M 77 | |
| Electrical performance | Test Condition | Test Method | TEIJIN SINGAPORE/L-1225L |
| Dielectric constant | ASTM D150/IEC 60250 | 2.9 | |
| optical performance | Test Condition | Test Method | TEIJIN SINGAPORE/L-1225L |
| Refractive index | ASTM D542/ISO 489 | 1.585 | |
| Transmittance rate | ASTM D1003/ISO 13468 | 88 % | |
| other | Test Condition | Test Method | TEIJIN SINGAPORE/L-1225L |
| purpose | 复合物 手机 开关 透明或半透明配件 | ||
| characteristic | 低粘度 脱模性良好 | ||
| thermal performance | Test Condition | Test Method | TEIJIN SINGAPORE/L-1225L |
| Vicat softening temperature | ASTM D1525/ISO R306 | 146 ℃(℉) | |
| Physical properties | Test Condition | Test Method | TEIJIN SINGAPORE/L-1225L |
| density | ASTM D792/ISO 1183 | 1.2 |