TPEE HTR8685 BK022A DUPONT USA
Hytrel®
Automotive Applications、Cable、Blow molding applications
High temperature resistan、Chemical resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | DUPONT USA/HTR8685 BK022A |
---|---|---|---|
Linear thermal expansion coefficient | MD | ISO11359-2 | 2.1E-04 cm/cm/°C |
TD | ISO11359-2 | 2E-04 cm/cm/°C | |
Melting Temperature | ISO11357-3 | 206 °C |
Elastomers Properties | Test Condition | Test Method | DUPONT USA/HTR8685 BK022A |
---|---|---|---|
Tearing Strength | 横向流量 | ISO34-1 | 110 kN/m |
流量 | ISO34-1 | 110 kN/m |
Hardness | Test Condition | Test Method | DUPONT USA/HTR8685 BK022A |
---|---|---|---|
Shore Hardness | 邵氏D,15秒 | ISO868 | 41 |
邵氏D | ISO868 | 44 |
Physical | Test Condition | Test Method | DUPONT USA/HTR8685 BK022A |
---|---|---|---|
Modeling Shrinkage | TD | ISO294-4 | 1.6 % |
MD | ISO294-4 | 1.7 % |
Mechanical Properties | Test Condition | Test Method | DUPONT USA/HTR8685 BK022A |
---|---|---|---|
Flexural Modulus | ISO178 | 100 Mpa | |
Tensile Stress | 10%应变 | ISO527-2 | 8.40 Mpa |
Tensile Strain | 断裂 | ISO527-2 | >300 % |
Nominal Tensile Strain at Break | ISO527-2 | 350 % | |
Tensile Stress | 断裂 | ISO527-2 | 30.0 Mpa |
Tensile Modulus | ISO527-2 | 100 Mpa | |
Tensile Stress | 50%应变 | ISO527-2 | 14.0 Mpa |
Flammability | Test Condition | Test Method | DUPONT USA/HTR8685 BK022A |
---|---|---|---|
Burning Rate | 1.00mm | ISO3795 | <100 mm/min |
FMVSS Flammability | FMVSS302 | B |