PA66 Alloy Orgalloy® RS 6635A ARKEMA FRANCE
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Electrical performance | Test Condition | Test Method | ARKEMA FRANCE/Orgalloy® RS 6635A |
---|---|---|---|
Volume resistivity | IEC 600932 | -- ohms·m | |
Dissipation Factor | 1MHz | IEC 602502 | -- |
relative permittivity | 1MHz | IEC 602502 | -- |
Compared to the Leakage Tracking Index (CTI) | IEC 601122 | ||
Surface Resistivity | IEC 600932 | -- ohms | |
Dissipation Factor | 100Hz | IEC 602502 | -- |
dielectric strength | IEC 60243-12 | 34 kV/mm | |
relative permittivity | 100Hz | IEC 602502 | -- |
Mechanical properties | Test Condition | Test Method | ARKEMA FRANCE/Orgalloy® RS 6635A |
---|---|---|---|
Tensile creep modulus | 1hr | ISO 899-12 | -- MPa |
Tensile modulus | ISO 527-22 | -- MPa | |
Tensile strain | 断裂 | ISO 527-22 | -- % |
Tensile creep modulus | 1000hr | ISO 899-12 | -- MPa |
tensile strength | 断裂 | ISO 527-22 | -- MPa |
flammability | Test Condition | Test Method | ARKEMA FRANCE/Orgalloy® RS 6635A |
---|---|---|---|
Burning Behav.atthicknessh | 3.20mm,UL | ISO 12102 | HB |
Burning Behav. | 1.60mm,UL | ISO 12102 | HB |
physical property | Test Condition | Test Method | ARKEMA FRANCE/Orgalloy® RS 6635A |
---|---|---|---|
Water absorption rate | 饱和 | ISO 622 | 1.7 % |
Melt volume flow rate | 275°C/2.16kg | ISO 11332 | 6.00 cm³/10min |
density | ISO 11832 | 1310 kg/m³ | |
Water absorption rate | 平衡 | ISO 622 | 0.70 % |
Thermal performance | Test Condition | Test Method | ARKEMA FRANCE/Orgalloy® RS 6635A |
---|---|---|---|
vicat | 50N | ISO 3062 | 200 °C |
Linear coefficient of thermal expansion | TD | ISO 11359-22 | 1E-04 cm/cm/°C |
MD | ISO 11359-22 | 1.7E-05 cm/cm/°C | |
Heat distortion temperature | 1.8MPa,HDT | ISO 75-22 | 225 °C |
0.45MPa,HDT | ISO 75-22 | 245 °C | |
melting temperature | ISO 11357-32 | 255 °C |