PP AX764 TPC SINGAPORE
COSMOPLENE® 
Thin-walled container、Electronic field、Electrical field
High rigidity、Impact copolymer、High mobility
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodTPC SINGAPORE/AX764
Impact strength of cantilever beam gap23°CASTM D25660 J/m
-20°CASTM D25637 J/m
hardnessTest ConditionTest MethodTPC SINGAPORE/AX764
Rockwell hardnessR级ASTM D78590
Mechanical propertiesTest ConditionTest MethodTPC SINGAPORE/AX764
elongation断裂ASTM D63850 %
tensile strength 断裂ASTM D63817.5 Mpa
屈服ASTM D63827.5 Mpa
Flexural modulusASTM D7901350 Mpa
flammabilityTest ConditionTest MethodTPC SINGAPORE/AX764
UL flame retardant ratingUL 94HB
physical property Test ConditionTest MethodTPC SINGAPORE/AX764
Shrinkage rateTD:2.00mm内部方法1.7 %
densityASTM D7920.900 g/cm³
melt mass-flow rateASTM D123850 g/10min
Shrinkage rateMD:2.00mm内部方法1.6 %
Thermal performanceTest ConditionTest MethodTPC SINGAPORE/AX764
Heat distortion temperature0.45MPa,未退火,HDTASTM D648122 °C