Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP JR-3070HP PRIME POLYMER JAPAN
PRIME POLYPRO
Food containers,Household goods
soft,High impact resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | PRIME POLYMER JAPAN/JR-3070HP |
---|---|---|---|
Rockwell hardness | R-Sale | ISO 2039-2 | 49 |
Basic Performance | Test Condition | Test Method | PRIME POLYMER JAPAN/JR-3070HP |
---|---|---|---|
density | ISO 1183 | 0.910 g/cm³ | |
melt mass-flow rate | 230℃ | ISO 1133 | 33 g/10min |
thermal performance | Test Condition | Test Method | PRIME POLYMER JAPAN/JR-3070HP |
---|---|---|---|
Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 65.0 °C |
0.45MPa | ISO 75 | 65 °C |
mechanical properties | Test Condition | Test Method | PRIME POLYMER JAPAN/JR-3070HP |
---|---|---|---|
Bending modulus | ISO 527 | 700 Mpa | |
elongation | Break | ISO 527 | 400 % |
Impact strength of cantilever beam gap | 23℃ | ISO 179 | 7.5 kJ/m² |
-20℃ | ISO 179 | 2.5 kJ/m² | |
Rockwell hardness | ISO 2039-2 | 49 R scale | |
Tensile modulus | ISO 527-2 | 700 Mpa | |
Tensile strain | Break | ISO 527-2 | 400 % |
tensile strength | Yield | ISO 527-2 | 20.0 Mpa |
ISO 527 | 20.0 Mpa |
Physical properties | Test Condition | Test Method | PRIME POLYMER JAPAN/JR-3070HP |
---|---|---|---|
melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 33 g/10min |
impact performance | Test Condition | Test Method | PRIME POLYMER JAPAN/JR-3070HP |
---|---|---|---|
Impact strength of simply supported beam without notch | -20°C | ISO 179 | 2.5 kJ/m² |
23°C | ISO 179 | 7.5 kJ/m² |