PPO(PPE) Norpex® AX270 EX Polymeric Resources Corporation (PRC)
--
currency
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

thermal performanceTest ConditionTest MethodPolymeric Resources Corporation (PRC)/Norpex® AX270 EX
Hot deformation temperature1.8MPa,UnannealedASTM D648129 °C
mechanical propertiesTest ConditionTest MethodPolymeric Resources Corporation (PRC)/Norpex® AX270 EX
Bending modulusASTM D7902410 MPa
elongationYieldASTM D63830 %
tensile strengthASTM D63863.4 MPa
Physical propertiesTest ConditionTest MethodPolymeric Resources Corporation (PRC)/Norpex® AX270 EX
densityASTM D7921.05 g/cm³
impact performanceTest ConditionTest MethodPolymeric Resources Corporation (PRC)/Norpex® AX270 EX
Impact strength of cantilever beam gap23°CASTM D256170 J/m