Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC LN-2250Y JIAXING TEIJIN
PANLITE®
Optical level、currency、Electrical components
Flame retardant、optical performance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Electrical performance | Test Condition | Test Method | JIAXING TEIJIN/LN-2250Y |
---|---|---|---|
Dissipation Factor | 23°C | IEC60250 | 1E-03 100HZ |
Dielectric Strength | IEC60243-1 | 32 KV/mm | |
IEC60093 | 1E+15 Ω.cm | ||
Dissipation Factor | 23°C | IEC60250 | 9E-03 1MHz |
dielectric constant | 23°C | IEC60250 | 3.00 1MHz |
Surface Resistivity | IEC60093 | 1E+15 Ω.cm | |
Dissipation Factor | 相对漏电起痕指数 | IEC60112 | 250 V |
Mechanical properties | Test Condition | Test Method | JIAXING TEIJIN/LN-2250Y |
---|---|---|---|
Tensile modulus | 23°C | ISO527-2 | 2400 Mpa |
Flexural modulus | 23°C | ISO178 | 2280 Mpa |
elongation at break | 23°C | ISO527-2 | 50 % |
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 19 kJ/m² |
bending strength | 23°C | ISO178 | 94.0 Mpa |
tensile strength | 23°C | ISO527-2 | 64.0 Mpa |
Flame retardant performance | Test Condition | Test Method | JIAXING TEIJIN/LN-2250Y |
---|---|---|---|
fire rating | UL-94 | 3.0mm V-0,5VB | |
UL-94 | 1.5mm V-0 |
physical property | Test Condition | Test Method | JIAXING TEIJIN/LN-2250Y |
---|---|---|---|
300℃/1.2Kg | ISO1133 | 11.0 cm3/10min | |
Shrinkage rate | MD2.0mm | ISO294-4 | 0.60 % |
Water absorption rate | (23°C,24hr) | ISO62 | 0.20 % |
Shrinkage rate | TD2.0mm | ISO294-4 | 0.60 % |
Thermal performance | Test Condition | Test Method | JIAXING TEIJIN/LN-2250Y |
---|---|---|---|
TD | ISO11359-2 | 7E-05 cm/cm/°C | |
0.45MPa未退火 | ISO75-2/Bf | 141 °C | |
1.80MPa退火 | ISO75-2/Af | 127 °C | |
vicat | ISO306/B50 | 148 °C | |
MD | ISO11359-2 | 7E-05 cm/cm/°C |