Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PA66 Nypol® PA A3 ST VRM0076 NR325 Brazil Petropol
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodBrazil Petropol/Nypol® PA A3 ST VRM0076 NR325
Impact strength of cantilever beam gap-40°CASTM D256180 J/m
23°CASTM D256990 J/m
-20°CASTM D256230 J/m
Mechanical propertiesTest ConditionTest MethodBrazil Petropol/Nypol® PA A3 ST VRM0076 NR325
elongation断裂ASTM D63875 %
tensile strength ASTM D63853.0 MPa
Flexural modulusASTM D7902200 MPa
flammabilityTest ConditionTest MethodBrazil Petropol/Nypol® PA A3 ST VRM0076 NR325
UL flame retardant ratingUL 94HB
physical property Test ConditionTest MethodBrazil Petropol/Nypol® PA A3 ST VRM0076 NR325
Shrinkage rateMDASTM D9551.5to1.7 %
Water absorption rate平衡ASTM D5701.2 %
densityASTM D7921.08to1.09 g/cm³
Thermal performanceTest ConditionTest MethodBrazil Petropol/Nypol® PA A3 ST VRM0076 NR325
Heat distortion temperature1.8MPa,未退火,HDTASTM D64865.0 °C
melting temperatureASTM D2117250to265 °C
Heat distortion temperature0.45MPa,未退火,HDTASTM D648225 °C
Linear coefficient of thermal expansionTD:23到55°CASTM D6961.3E-04 cm/cm/°C
MD:23到55°CASTM D6961.4E-04 cm/cm/°C