Thermal Properties | Test Condition | Test Method | DUPONT USA/HTN51G35HSLR |
---|---|---|---|
Heat Deflection Temperature | 0.45MPa,未退火 | ISO75-2/B | 284 °C |
Linear thermal expansion coefficient | TD:-- | ISO11359-2 | 5.5E-05 cm/cm/°C |
Heat Deflection Temperature | 1.8MPa,未退火 | ISO75-2/A | 260 °C |
Melting Temperature | ISO11357-3 | 300 °C | |
Linear thermal expansion coefficient | MD:-40to23°C | ISO11359-2 | 1.8E-05 cm/cm/°C |
MD:-- | ISO11359-2 | 1.8E-05 cm/cm/°C | |
TD:-40to23°C | ISO11359-2 | 5.5E-05 cm/cm/°C |
Hardness | Test Condition | Test Method | DUPONT USA/HTN51G35HSLR |
---|---|---|---|
Rockwell Hardness | M计秤 | ISO2039-2 | 108 |
R计秤 | ISO2039-2 | 124 |
Additional | Test Condition | Test Method | DUPONT USA/HTN51G35HSLR |
---|---|---|---|
Odor | VDA270 | 4.00 |
Physical | Test Condition | Test Method | DUPONT USA/HTN51G35HSLR |
---|---|---|---|
SpecificHeatCapacityofMelt | 1860 J/kg/°C | ||
Moisture Absorption | 饱和,23°C,2.00mm | ISO62 | 4.5 % |
Modeling Shrinkage | TD | ISO294-4 | 0.60 % |
MD | ISO294-4 | 0.20 % | |
ThermalConductivityofMelt | 0.25 W/m/K |
Mechanical Properties | Test Condition | Test Method | DUPONT USA/HTN51G35HSLR |
---|---|---|---|
Flexural Modulus | ISO178 | 10300 Mpa | |
Tensile Creep Modulus | 1000hr | ISO899-1 | -- Mpa |
Poisson Ratio | ISO527 | 0.39 | |
Tensile Strain | 断裂 | ISO527-2 | 2.4 % |
Tensile Stress | 断裂 | ISO527-2 | 210 Mpa |
Flexural Stress | ISO178 | 300 Mpa | |
Tensile Modulus | ISO527-2 | 12000 Mpa | |
Tensile Creep Modulus | 1hr | ISO899-1 | -- Mpa |
Impact Properties | Test Condition | Test Method | DUPONT USA/HTN51G35HSLR |
---|---|---|---|
Charpy Unnotched Impact Strength | 23°C | ISO179/1eU | 70 kJ/m² |
-30°C | ISO179/1eU | 60 kJ/m² |
Flammability | Test Condition | Test Method | DUPONT USA/HTN51G35HSLR |
---|---|---|---|
Burning Rate | 1.00mm | ISO3795 | 23 mm/min |
FMVSS Flammability | FMVSS302 | B | |
Flame Rating | 0.9mm | UL94 | HB |
Oxygen Index | ISO4589-2 | 24 % | |
Flame Rating | 1.5mm | UL94 | HB |
0.9mm | IEC60695-11-10,-20 | HB | |
1.5mm | IEC60695-11-10,-20 | HB |
Electrical Properties | Test Condition | Test Method | DUPONT USA/HTN51G35HSLR |
---|---|---|---|
Dielectric Strength | IEC60243-1 | 36 KV/mm | |
Volume Resistivity | IEC60093 | >1.0E+15 ohms·cm | |
Comparative Tracking Index | IEC60112 | 600 V | |
Surface Resistivity | IEC60093 | -- ohms | |
Relative Permittivity | 1MHz | IEC60250 | 4.00 |
100Hz | IEC60250 | 4.00 |