| thermal performance | Test Condition | Test Method | BASF GERMANY/B 4040 G10 BK |
|---|---|---|---|
| Melting temperature | ISO 3146 | 223 °C | |
| Hot deformation temperature | 0.45MPa,Unannealed | ASTM D648 | 220 °C |
| Melting temperature | ASTM D3418 | 223 °C | |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 221 °C |
| 1.8MPa,Unannealed | ASTM D648 | 215 °C | |
| Linear coefficient of thermal expansion | MD | 2.5E-05 cm/cm/°C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 205 °C |
| impact performance | Test Condition | Test Method | BASF GERMANY/B 4040 G10 BK |
| Impact strength of simply supported beam without notch | -30°C | ISO 179 | 69 kJ/m² |
| 23°C | ISO 179 | 52 kJ/m² | |
| Physical properties | Test Condition | Test Method | BASF GERMANY/B 4040 G10 BK |
| Melt Volume Flow Rate (MVR) | 275°C/2.16kg | ISO 1133 | 6.00 cm3/10min |
| Viscosity value | 降低的粘度 | ISO 1628 | 97.0 ml/g |
| Water absorption rate | Equilibrium,50%RH | ASTM D570 | 0.12 % |
| Equilibrium,23°C,50%RH | ISO 62 | 0.12 % | |
| Saturation,23°C | ISO 62 | 0.40 % | |
| Shrinkage rate | MD:3.18mm | 0.20 % | |
| Water absorption rate | Saturation | ASTM D570 | 0.40 % |
| Electrical performance | Test Condition | Test Method | BASF GERMANY/B 4040 G10 BK |
| Dielectric constant | 100Hz | IEC 60250 | 4.00 |
| Dissipation factor | 100Hz | IEC 60250 | 1.2E-03 |
| Volume resistivity | 1.50mm | ASTM D257 | >1.0E+15 ohms |
| IEC 60093 | >1.0E+15 ohms·cm | ||
| Dissipation factor | 1MHz | IEC 60250 | 0.015 |
| Surface resistivity | IEC 60093 | 1E+13 ohms | |
| Dielectric constant | 1MHz | IEC 60250 | 4.00 |
| mechanical properties | Test Condition | Test Method | BASF GERMANY/B 4040 G10 BK |
| Bending modulus | 23°C | ASTM D790 | 13600 Mpa |
| bending strength | 23°C | ISO 178 | 225 Mpa |
| tensile strength | Break,23°C | ISO 527-2 | 155 Mpa |
| Break,23°C | ASTM D638 | 140 Mpa | |
| Bending modulus | 23°C | ISO 178 | 15000 Mpa |
| elongation | Break,23°C | ASTM D638 | 1.5 % |
| Tensile modulus | 23°C | ISO 527-2 | 16500 Mpa |
| Tensile strain | Break,23°C | ISO 527-2 | 1.5 % |