| thermal performance | Test Condition | Test Method | TAIWAN GINAR/A1520NH B06 |
|---|---|---|---|
| Melting temperature | ASTM D789 | 260 °C | |
| Hot deformation temperature | 1.8 MPa, Unannealed | ASTM D648 | 245 °C |
| mechanical properties | Test Condition | Test Method | TAIWAN GINAR/A1520NH B06 |
| elongation | Break | ASTM D638 | > 1.5 % |
| bending strength | ASTM D790 | 214 Mpa | |
| tensile strength | Yield | ASTM D638 | 137 Mpa |
| Bending modulus | ASTM D790 | 7580 Mpa | |
| flammability | Test Condition | Test Method | TAIWAN GINAR/A1520NH B06 |
| UL flame retardant rating | 0.8 mm | UL 94 | V-0 |
| 1.6 mm | UL 94 | V-0 | |
| 3.2 mm | UL 94 | V-0 | |
| Physical properties | Test Condition | Test Method | TAIWAN GINAR/A1520NH B06 |
| melt mass-flow rate | 275°C/5.0 kg | ASTM D1238 | 40 to 80 g/10 min |
| Shrinkage rate | 3.00 mm,Flow | ASTM D955 | 0.25 - 0.45 % |