AS(SAN) 368R INEOS STYRO THAILAND
Luran®
Monitor、Pen、Household goods、Electrical appliances、Toothbrush handle
transparent、Good stability
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | INEOS STYRO THAILAND/368R |
---|---|---|---|
Impact strength of simply supported beam without notch | 23°C | ISO179 | 18 kJ/m² |
-30°C | ISO179 | 18 kJ/m² |
hardness | Test Condition | Test Method | INEOS STYRO THAILAND/368R |
---|---|---|---|
ISO2039-1 | 165 Mpa | ||
Rockwell hardness | M级 | 83 |
Electrical performance | Test Condition | Test Method | INEOS STYRO THAILAND/368R |
---|---|---|---|
Surface Resistivity | IEC60093 | >1.0E+15 ohms | |
Dissipation Factor | 100Hz | IEC60250 | 4E-03 |
Volume resistivity | IEC60093 | 1E+16 ohms·cm | |
dielectric constant | 100Hz | IEC60250 | 3.00 |
Dissipation Factor | 1MHz | IEC60250 | 7E-03 |
Mechanical properties | Test Condition | Test Method | INEOS STYRO THAILAND/368R |
---|---|---|---|
TensileCreepModule | 1hr | ISO899-1 | 3500 Mpa |
Bending stress | ISO178 | 125 Mpa | |
Tensile modulus | ISO527-2 | 3700 Mpa | |
Tensile stress | 屈服,23°C | ISO527-2 | 75.0 Mpa |
Tensile strain | 断裂,23°C | ISO527-2 | 3.0 % |
Tensile creep modulus | 1000hr | ISO899-1 | 2800 Mpa |
optical performance | Test Condition | Test Method | INEOS STYRO THAILAND/368R |
---|---|---|---|
refractive index | ISO489 | 1.569 | |
Haze ratio | ASTMD1003 | <1.0 % | |
transmissivity | 550nm | ASTMD1003 | >89.0 % |
physical property | Test Condition | Test Method | INEOS STYRO THAILAND/368R |
---|---|---|---|
Water absorption rate | 平衡,23°C,50%RH | ISO62 | 0.20 % |
Apparent density | 0.65 g/cm³ | ||
Melt volume flow rate | 220°C/10.0kg | ISO1133 | 10.0 cm3/10min |
Shrinkage rate | ISO294-4 | 0.30to0.70 % |
Thermal performance | Test Condition | Test Method | INEOS STYRO THAILAND/368R |
---|---|---|---|
Hot deformation temperature 3 | 0.45MPa,Annealed | ISO75-2/B | 100 °C |
thermal conductivity | DIN52612 | 0.17 W/m/K | |
vicat | ISO306/B50 | 106 °C | |
Hot deformation temperature 3 | 1.8MPa,Annealed | ISO75-2/A | 88.0 °C |
MD | ISO11359-2 | 7E-05 cm/cm/°C |