ABS EXCELLOY EK50 Techno Polymer Co, Ltd.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Techno Polymer Co, Ltd./EXCELLOY EK50 |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | 12 kJ/m² | |
Impact strength of cantilever beam gap | ASTM D256 | 120 J/m |
hardness | Test Condition | Test Method | Techno Polymer Co, Ltd./EXCELLOY EK50 |
---|---|---|---|
Rockwell hardness | R计秤 | ISO 2039-2 | 98 |
R级 | ASTM D785 | 100 |
Mechanical properties | Test Condition | Test Method | Techno Polymer Co, Ltd./EXCELLOY EK50 |
---|---|---|---|
bending strength | -- | ASTM D790 | 68.6 MPa |
Flexural modulus | -- | ISO 178 | 2000 MPa |
tensile strength | 屈服 | ASTM D638 | 39.2 MPa |
屈服 | ISO 527-2 | 41.0 MPa | |
bending strength | -- | ISO 178 | 64.0 MPa |
Flexural modulus | -- | ASTM D790 | 2350 MPa |
Electrical performance | Test Condition | Test Method | Techno Polymer Co, Ltd./EXCELLOY EK50 |
---|---|---|---|
Surface Resistivity | ASTM D257 | 3E+10 ohms | |
Compared to the Leakage Tracking Index (CTI) | JISL1094 | PLC 3 |
flammability | Test Condition | Test Method | Techno Polymer Co, Ltd./EXCELLOY EK50 |
---|---|---|---|
UL flame retardant rating | ALL | UL 94 | HB |
physical property | Test Condition | Test Method | Techno Polymer Co, Ltd./EXCELLOY EK50 |
---|---|---|---|
Shrinkage rate | ISO 294-4 | 0.40to0.60 % | |
density | ISO 1183 | 1.07 g/cm³ | |
melt mass-flow rate | 220°C/10.0kg | ISO 1133 | 15 g/10min |
Thermal performance | Test Condition | Test Method | Techno Polymer Co, Ltd./EXCELLOY EK50 |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ASTM D648 | 100 °C |
0.45MPa,未退火,HDT | ISO 75-2/B | 87.0 °C |