Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

Epoxy Epoxies, Ect. 20-3236 Epoxies, Etc.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Supplementary Information | Test Condition | Test Method | Epoxies, Etc./Epoxies, Ect. 20-3236 |
|---|---|---|---|
| operate temperature | -55.0-120 °C | ||
| WeightLossonHeating-After | 0.64 |
| Uncured Properties | Test Condition | Test Method | Epoxies, Etc./Epoxies, Ect. 20-3236 |
|---|---|---|---|
| Color | Amber | ||
| Curing time | 25°C | 24to36 hr | |
| Shelf Life | 6 month | ||
| 45°C | 6.0to8.0 hr | ||
| 65°C | 2.0to3.0 hr | ||
| Pot Life2(25°C) | 300 min | ||
| MixRatiobyWeight(PBW) | PartB | 1.0 | |
| 密度1(25°C) | 1.07 g/cm³ | ||
| PartA | 2.0 |
| thermosetting | Test Condition | Test Method | Epoxies, Etc./Epoxies, Ect. 20-3236 |
|---|---|---|---|
| Thermosetting mixed viscosity | 25°C | 3000 cP |
| Cured Properties | Test Condition | Test Method | Epoxies, Etc./Epoxies, Ect. 20-3236 |
|---|---|---|---|
| Dissipation factor | 1MHz | 0.021 | |
| elongation | Break | 6.4 % | |
| Relative permittivity | 1MHz | 3.57 | |
| Shore hardness | ShoreD | 80 | |
| tensile strength | 57.2 MPa | ||
| Water absorption rate | 0.21 % |
| impact performance | Test Condition | Test Method | Epoxies, Etc./Epoxies, Ect. 20-3236 |
|---|---|---|---|
| Impact strength of cantilever beam gap | 29 J/m |