Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PPS+PPE XYRON™ DG043 ASAHI JAPAN
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | ASAHI JAPAN/XYRON™ DG043 |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | 2.0 kJ/m² |
Mechanical properties | Test Condition | Test Method | ASAHI JAPAN/XYRON™ DG043 |
---|---|---|---|
Tensile strain | 断裂 | ISO 527-2 | 2.0 % |
tensile strength | 屈服 | ISO 527-2 | 79.0 MPa |
Flexural modulus | ISO 178 | 9770 MPa | |
bending strength | ISO 178 | 132 MPa |
Electrical performance | Test Condition | Test Method | ASAHI JAPAN/XYRON™ DG043 |
---|---|---|---|
dielectric constant | 100Hz | IEC 60250 | 4.00 |
Volume resistivity | IEC 60093 | 1E+16 ohms·cm | |
Dissipation Factor | 100Hz | IEC 60250 | 1E-03 |
dielectric strength | 2.00mm | IEC 60243-1 | 29 kV/mm |
dielectric constant | 1MHz | IEC 60250 | 4.00 |
Surface Resistivity | IEC 60093 | 1E+16 ohms | |
Dissipation Factor | 1MHz | IEC 60250 | 2E-03 |
flammability | Test Condition | Test Method | ASAHI JAPAN/XYRON™ DG043 |
---|---|---|---|
UL flame retardant rating | 0.75mm | UL 94 | V-1 |
1.5mm | UL 94 | V-0 |
physical property | Test Condition | Test Method | ASAHI JAPAN/XYRON™ DG043 |
---|---|---|---|
Shrinkage rate | 2.00mm | 内部方法 | 0.15to0.30 % |
density | ISO 1183 | 1.52 g/cm³ |
Thermal performance | Test Condition | Test Method | ASAHI JAPAN/XYRON™ DG043 |
---|---|---|---|
Linear coefficient of thermal expansion | MD:-30到65°C | ISO 11359-2 | 3E-05 cm/cm/°C |
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 185 °C |