thermal performance | Test Condition | Test Method | SABIC INNOVATIVE US/KB-1006 |
---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed,3.20mm | ASTM D648 | 103 °C |
0.45MPa,Unannealed,64.0mmSpan | ISO 75-2/Bf | 152 °C | |
1.8MPa,Unannealed,64.0mmSpan | ISO 75-2/Af | 107 °C | |
0.45MPa,Unannealed,3.20mm | ASTM D648 | 155 °C | |
Linear coefficient of thermal expansion | TD:-30to30°C | ASTM D696 | 8.3E-05 cm/cm/°C |
MD:-30to30°C | ASTM D696 | 8.3E-05 cm/cm/°C |
mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE US/KB-1006 |
---|---|---|---|
Bending modulus | 50.0mmSpan | ASTM D790 | 4000 Mpa |
ISO 178 | 4320 Mpa | ||
bending strength | Break,50.0mmSpan | ASTM D790 | 43.0 Mpa |
ISO 178 | 65.0 Mpa | ||
elongation | Break | ASTM D638 | 20 % |
Tensile strain | Break | ISO 527-2/5 | 20 % |
tensile strength | Break | ISO 527-2/5 | 37.0 Mpa |
Break | ASTM D638 | 34.0 Mpa |
Physical properties | Test Condition | Test Method | SABIC INNOVATIVE US/KB-1006 |
---|---|---|---|
Shrinkage rate | TD:24hr | ASTM D955 | 1.0-3.0 % |
MD:24hr | ASTM D955 | 1.0-3.0 % | |
Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.20 % |
24hr,50%RH | ASTM D570 | 0.20 % |
impact performance | Test Condition | Test Method | SABIC INNOVATIVE US/KB-1006 |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 4.5 kJ/m² |
Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 25 kJ/m² |