Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPU A85P4854 HUNTSMAN GERMANY
IROGRAN®
--
High elasticity,Easy to process,wear resistant,Weather resistance,Hydrolysis resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | HUNTSMAN GERMANY/A85P4854 |
|---|---|---|---|
| Shore hardness | ShoreA,Injection | ASTM D2240 | 83 |
| ShoreA,Injection | ISO 868 | 83 | |
| ShoreD,Injection | ISO 868 | 33 | |
| ShoreD,Injection | ASTM D2240 | 33 |
| thermal performance | Test Condition | Test Method | HUNTSMAN GERMANY/A85P4854 |
|---|---|---|---|
| TMA | High:635.0μm | Internal Method | 180 °C |
| Low:635.0μm | Internal Method | 125 °C |
| mechanical properties | Test Condition | Test Method | HUNTSMAN GERMANY/A85P4854 |
|---|---|---|---|
| Wear resistance | ISO 4649 | 40 mm³ |
| Physical properties | Test Condition | Test Method | HUNTSMAN GERMANY/A85P4854 |
|---|---|---|---|
| Melt Volume Flow Rate (MVR) | 190°C/21.6kg | 150 cm3/10min | |
| Shrinkage rate | MD:Injection | ASTM D955 | 0.80 % |
| flammability | Test Condition | Test Method | HUNTSMAN GERMANY/A85P4854 |
|---|---|---|---|
| UL flame retardant rating | UL 94 | V-0 |
| elastomer | Test Condition | Test Method | HUNTSMAN GERMANY/A85P4854 |
|---|---|---|---|
| elongation | Break | DIN 53504 | 670 % |
| Break | ASTM D412 | 670 % | |
| tear strength | ISO 34-1 | 35 kN/m | |
| ASTM D624 | 35.0 kN/m | ||
| tensile strength | Break | ASTM D412 | 25.0 Mpa |
| 300%Strain | DIN 53504 | 7.50 Mpa | |
| Break | DIN 53504 | 25.0 Mpa | |
| 100%Strain | ASTM D412 | 3.50 Mpa | |
| 300%Strain | ASTM D412 | 7.50 Mpa | |
| 100%Strain | DIN 53504 | 3.50 Mpa |